Table 5: Comparison of the results with Tan’s results: a) IJT-BGJ-1 vs T23, and b) IJT-BGJ-2 vs T25.

(a) (b)
Comparison Variable Exp. Result Tan (2009) Comparison Variable Exp. Result Tan (2009)
Thickness of Gusset Plate 10 mm 6 mm Thickness of Gusset Plate 10 mm 6 mm
Depth of Column 300 mm 250 mm Depth of Column 300 mm 250 mm
Test Label IJT-BGJ-1 T23 Test Label IJT-BGJ-2 T25
Mj(Exp) (kNm) 27.64 14.27 Mj(Exp) (kNm) 30.37 22.74
Mj(The) (kNm) 20.6 13.12 Mj(The) (kNm) 22.4 20.5
Sj (Exp) (kNm/rad) 260 245 Sj (Exp) (kNm/rad) 570 553
Sj (The) (kNm/rad) 637 470 Sj (The) (kNm/rad) 892 744